MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Marfak® Multipurpose NLGI Grade 2
Categories: Fluid; Lubricant; Lithium Gellant; Organic Soap Gellant

Material Notes: Texaco Marfak Multipurpose delivers value through:
  • Good water resistance — Provides lubrication in the presence of water.
  • Good corrosion protection — Inhibited to protect gear and bearing surfaces.
  • Good oxidation stability — Helps to ensure long life in storage and in use.
  • Simplified lubrication — One grease designed to satisfy most general purpose, non-EP grease requirements.

Texaco Marfak Multipurpose is manufactured using selected, highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thickener, and rust and oxidation inhibitors.

It is work stable and resists separation or throw out from antifriction bearings. It has a low oil bleeding tendency under pressure and is pumpable at low temperatures.

Texaco Marfak Multipurpose satisfies general automotive and industrial applications that do not require the use of an EP grease.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.
  2. Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.
  3. Determined on mineral oil extracted by vacuum filtration.

CPS Number: 220958; MSDS Number: 8962

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Saybolt Viscosity at 100°F 1200 SUSSee Note 3.
Saybolt Viscosity at 210°F 93 SUSSee Note 3.
Kinematic Viscosity at 40°C (104°F) 220 cStSee Note 3.
Kinematic Viscosity at 100°C (212°F) 18.1 cStSee Note 3.
 
Mechanical PropertiesOriginal ValueComments
Penetration P(60), 1/10 mm 280Unknown Amount of Work, 25°C (77°F)
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °CSee Note 2.
Minimum Service Temperature, Air -20.0 °CSee Note 1.
Pour Point -12.0 °CSee Note 3.
Flash Point 198 °CSee Note 3.
Dropping Point 188 °C
 
Descriptive Properties
ColorBrown
Corrosion, Copper Strip1B
TextureButtery
Thickener, %7.5Lithium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WTEXA250 / 77129

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.