MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ASI® MP 54190 GR Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: MP 54190 GR is a medium viscosity polyamide/epoxy adhesive recommended for bonding applications where high shock impact resistance and peel resistance are desired. This 1 : 1 ratio, two part adhesive is easily mixed and cured at room temperature and develops tough, strong bonds to a wide variety of materials, including metals, glass, ceramics and plastics. Fully cured MP 54190 GR bonds offer superior thermal shock resistance, mechanical, electrical, electrical and impact dimensional stability and resistance to water, weather, oxygen and ozone, most petroleum products, mild acids and alkalis and many other chemicals.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/cc
Viscosity 60000 cP
@Temperature 25.0 °C
mixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 460 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 58.0 µm/m-°C
Maximum Service Temperature, Air 110 °C
Minimum Service Temperature, Air -60.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 65.0 °C
 48.0 hour
@Temperature 25.0 °C
Pot Life 20.0 - 40.0 min
@Temperature 25.0 °C
Shelf Life 12.0 Month
@Temperature <=32.2 °C
Out of sunlight and in original sealed containers.
 
Descriptive Properties
Color / appearancetransparent / gray
Mix Ratio100:100 (resin: hardener)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASINC9090 / 233457

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.