MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lanxess LEWATIT® VP OC 1064 MD PH Macroporous Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® VP OC 1064 MD PH is a macroporous adsorber resin without functional groups. It has a very good chemical and mechanical stability and beads of uniform size (monodisperse). Lewatit VP OC 1064 MD PH is suitable for removing and adsorbing the following ingredients in the following ingredients in the chemical pharmaceutical industry (e.g. from waste water or from product streams):
  • Anionic, cationic and non-ionic surfactants
  • Chlorinated and nitrated hydrocarbons
  • Colorants or organic inert materials
  • Residual amounts of the liquid extraction agents, such as tributyl phosphate and Di-2-Ethyhexl phosphate
  • Non-polar organic ingredients with low molecular mass
Lewatit VP OC 1064 MD PH has the following properties:
  • a very high mechanical stability
  • a longer resin life time and better regeneration efficiency compared to activated carbon
  • a high adsorption capacity especially at medium and high feed concentration
  • a good kinetic performance during adsorption and elution.
Prior to industrial application, preliminary test should be carried out on a laboratory scale, in order to determine the maximum adsorptive capacity and the optimum regenerant. Experience has shown that the end capacity of the adsorber resin is reached after the third cycle.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.600 g/cc
Density 1.02 g/cc
Bead Size 0.440 - 0.540 mmMean
Storage Temperature -20.0 - 40.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °C
 
Descriptive Properties
AppearanceWhite, opaque
pH Operating Range1 - 14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8861 / 209253

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.