SABIC® PPcompound 7990E is a mineral filled modified polypropylene. This material combines a very high flow with a high stiffness, it has been optimized for minimized VOC and FOG. Typical applications include non esthetical automotive interior parts and multi material injection molding (textile overmolding) such as door panels and interior trim.
SABIC® PPcompound 7990E is a designated automotive grade.
IMDS ID: 62454794Information provided by SABIC |