MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
ExxonMobil LDPE LD 252 Low Density Polyethylene Resin (European Grade)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: LD 525 is a high purity LDPE extrusion coating grade, designed to meet environmental needs for reduced fume emissions during plastics conversion. This grade offers:
  • Low volatiles level, resulting in reduced fume emissions during extrusion at high temperatures (up to 20% reduction versus standard LDPE)
  • Excellent neck-in/draw down balance, resulting in low edge trim ie less waste.
  • Outstanding barrier characteristics especially for water vapor, e.g. for applications in portion packaging (sugar, salt…)
  • Good organoleptic properties, i.e. low off-taste and odor.
Availability: Africa & Middle East and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: No
Applications:
  • Coextrusion Coating
  • Extrusion Coating
  • Extrusion Lamination
  • Food packaging
  • Industrial Packaging
  • Liquid Packaging

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccExxonMobil method
Melt Flow 3.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Neck In 1.60 in
@Temperature 315 °C
492 ft/min, Constant output at 35 rpm; ExxonMobil Method
 1.70 in
@Temperature 315 °C
328 ft/min, Constant output at 35 rpm; ExxonMobil Method
Drawdown 4.50 m/s
@Temperature 315 °C
Constant output at 35 rpm; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 228 °FPeak Melting Point; ExxonMobil method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEX99277 / 175513

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.