Description: Hostaform® Acetal Copolymers are a high strength, crystalline, thermoplastic engineering resins whose balance of properties and ease of processability offer performance and cost advantages over many other materials. Specific Notes for this Grade: Extrusion blow molding grade. Stiff-flowing, high melt strength. Also for injection molding of thick-walled, void-free parts. Information provided by Celanese Corporation. |