MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Chirulen® 1020 HXLPE MediTECH Compression Molded and Irradiated UHMWPE Form  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: MediTECH Compression Molded and Irradiated UHMWPE Form, produced from Celanese GUR 1020 resin. Chirulen® 1020, 75 kGy, Above Melt Annealed materials maintain the toughness of UHMWPE, while providing the enhanced wear properties of the more highly crosslinked polymer, with the stability provided by the above melt annealing for free radical neutralization. ISO Cell Designation: Thermoplastic ISO 11542-PE-UHMW QD, 2-2-2, ASTM Cell Designation: S-UHMW-PE0111A111 Material evaluated based on ISO 5834-1 Type 1, ISO 5834-2 Type 1, and ASTM F648 Type 1.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.931 g/ccCrosslinked Fabricated Form; ASTM D792
 0.935 g/ccAnnealed Fabricated Form Prior to Crosslinking; ASTM D792
Water Absorption <= 0.050 %until saturation, Annealed Fabricated Form Prior to Crosslinking; ASTM D570
 <= 0.050 %until saturation, Crosslinked Fabricated Form; ASTM D570
Oxidative Induction Time (OIT) 10 min
@Temperature 200 °C
Annealed Fabricated Form Prior to Crosslinking; ASTM D3895
Crystallinity 53 %1st heat, 20°C - 160°C, Crosslinked Fabricated Form; ASTM F2625
 58 %1st heat, 20°C - 160°C, Annealed Fabricated Form Prior to Crosslinking; ASTM F2625
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 66
@Time 15.0 sec
Annealed Fabricated Form Prior to Crosslinking; ASTM D2240
Tensile Strength, Ultimate 52.0 MPaCrosslinked Fabricated Form; ASTM F648 /ASTM D638
 57.2 MPaAnnealed Fabricated Form Prior to Crosslinking; ASTM F648 /ASTM D638
Tensile Strength, Yield 20.6 MPaCrosslinked Fabricated Form; ASTM F648 /ASTM D638
 21.7 MPaAnnealed Fabricated Form Prior to Crosslinking; ASTM F648 /ASTM D638
Elongation at Break 350 %Crosslinked Fabricated Form; ASTM F648 /ASTM D638
 474 %Annealed Fabricated Form Prior to Crosslinking; ASTM F648 /ASTM D638
Compressive Modulus 792 MPaCrosslinked Fabricated Form; ASTM D792
Charpy Impact Unnotched 196 kJ/m²ISO 11542-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear 180 µm/m-°C
@Temperature 23.0 - 80.0 °C
Annealed Fabricated Form Prior to Crosslinking; ASTM D696
Thermal Conductivity 0.400 W/m-KAnnealed Fabricated Form Prior to Crosslinking; DIN 52612
Melting Point 135.7 °C10°C / min, Crosslinked Fabricated Form; ASTM DF2625
 136 °C10°C / min, Annealed Fabricated Form Prior to Crosslinking; ASTM DF2625
Crystallization Temperature 126 - 144 °CAnnealed Fabricated Form Prior to Crosslinking; ASTM F2625
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °CAnnealed Fabricated Form Prior to Crosslinking; ASTM D648
Vicat Softening Point 134 °C
@Load 1.02 kg
50 °C/Hr., Annealed Fabricated Form Prior to Crosslinking; ASTM D1525 B
 
Descriptive Properties
Determination of Network Parameters of Crosslinking0.021[Ratio], Trans Vinylene Yield by Infrared Spectroscopy for Cross Link Density, ASTM F2381
 0.17 mol/dm^3In Situ Crosslink Density, ASTM F2214
 3.3[Ratio], In Situ Swell Ratio, ASTM F2214
 5266 g/molIn Situ Molecular Weight between Crosslinks, ASTM F2214
 Below RL[Spins / gram], Electron Spin Resonance
Fatigue Crack Propagation Properties1.196MPa*m^1/2, ?K inception
 2.18E-08[mm/cycle], C (Y Intercept) Linear Region
 5.865for ?K in MPa*m^1/2, m (exponent) Linear Region
 8.36for ?K in MPa*m^1/2, m (exponent) 1x10-7 to 2x10-4
 8.83E-09[m/cycle/(Map*m^1/2)^m)], C (Y Intercept) 1x10-7 to 2x10-4
Oxidation Properties<0.1Surface Oxidative Index, Time = 0, ASTM F2102
 <0.1Bulk Oxidative Index, Time = 0, ASTM F2102
 <0.1Maximum Oxidative Index, Time = 0, ASTM F2102
 0.1Surface Oxidative Index, Time = 2 weeks, ASTM F2102 /ASTM F2003
 0.1Bulk Oxidative Index, Time = 2 weeks, ASTM F2102 /ASTM F2003
 0.1Maximum Oxidative Index, Time = 2 weeks, ASTM F2102 /ASTM F2003
Oxidation Resistance<0.1ASTM F2102, Surface Oxidation Index, Annealed Fabricated Form Prior to Crosslinking
 <0.1ASTM F2102, Bulk Oxidation Index, Annealed Fabricated Form Prior to Crosslinking
 <0.1ASTM F2102, Surface Oxidation Index, Crosslinked Fabricated Form
 <0.1ASTM F2102, Bulk Oxidation Index, Crosslinked Fabricated Form
Small Punch Properties184.4-283.6 mJWork to Failure, ASTM F2183
 4.196 mmMaximum Displacement, ASTM F2183
 70.05 NNominal Yield, ASTM F2183
 79.37 NMaximum Load, ASTM F2183

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

P1SM930 / 291087

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.