MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman n-Butanol Solvent
Categories: Fluid; Solvent

Material Notes: CAS No. 71-36-3

Product Description: Eastman™ n-Butanol (n-Butyl alcohol), a four carbon straight chain oxo alcohol, is a mediumboiling liquid that is useful as a chemical intermediate and as a solvent for ambient dry and baking coatings. It is widely used as an etherification alcohol in the manufacture of amino resins that are used as curing agents in baking and physical-drying finishes. Eastman™ n-Butanol is also a very effective latent solvent for cellulosic lacquers and ambient-cured enamels, reducing formulation viscosity and providing excellent flow and leveling during film formation. The chemical substances for this product are listed as Inert Ingredients Permitted for Use in Nonfood Use Pesticide Products, and in Food Use Pesticide Products with limitations, under the Federal Insecticide, Fungicide, and Rodenticide Act (FIFRA).

Application/Uses:

  • Chemical Intermediate - Acrylates, Ester Solvents, Glycol Ethers, Plasticizers
  • Coatings - Automotive OEM
  • Coatings - Automotive Refinish
  • Coatings - Can and Coil
  • Coatings - General Industrial
  • Coatings - Industrial Maintenance and Marine
  • Coatings - Industrial Wood
  • Coatings - Misc. (Thinners and Purge Solvents)
  • Coatings - Transportation
Key Attributes:
  • Excellent reactivity as an intermediate
  • Improves flow and gloss in cellulose lacquers and amino baking finishes
  • Inert - Food use with limitations
  • Inert - Nonfood use
  • Latent solvent in cellulose lacquers
  • Non-HAP
  • Readily biodegradable
  • Slow evaporation rate

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.810 g/cc
Viscosity 3.0 cPLiquid
Molecular Weight 74.12 g/mol
Vapor Pressure 0.00724 atm
@Temperature 20.0 °C
 0.0602 atm
@Temperature 55.0 °C
Surface Tension 24.6 dynes/cm
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 43.7 atm
Critical Temperature 289.8 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
Melting Point -89.0 °CFreezing Point
Boiling Point 116 - 119 °C@ 760 mm Hg
Flash Point 6.00 °CTag Closed Cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.40
 
Descriptive Properties
ColorPt-Co

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5252 / 222446

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.