MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Master Bond MB295 Cyanoacrylate Adhesive System
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Master Bond Polymer System MB295 is an ethyl cyanoacrylate adhesive system, recommended for use for combinations of plastics, lubber, ceramic or glass. Provides better general resistance to effects of extreme humidity.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.05 g/cc
Viscosity 1300 - 1700 cP
@Temperature 23.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.6
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 195 °F
Minimum Service Temperature, Air -60.0 °F
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.47
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month35-45°F
 
Descriptive Properties
ColorTransparent
Set-Up Time, minutes0.33-0.66At Room Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond LTX 123 Water-Borne Aliphatic Urethane Adhesive
Master Bond LTX 119 Pressure Sensitive Acrylic Adhesive Latex Compound

PMASTB206 / 52363

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.