MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
BASF Ultraform® N 2720 M210 AT POM, 10% Mineral Reinforced
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Mineral Filled

Material Notes: Product Description: Ultraform® N 2720 M210 AT is a 10% mineral reinforced injection molding POM grade with good wear properties for low-warpage parts with enhanced stiffness, strength and hardness. Typical applications include conveyor belts and transportation systems.

Availability: North America

Filler/Reinforcement: Mineral, 10% Filler by Weight

Features: Good Hardness; Good Stiffness; Good Strength; Low Warpage; Wear Resistant

Use: Belts/Belt Repair

Agency Ratings: EC 1907/2006 (REACH)

RoSH Compliance: RoSH Compliant

Processing Method: Injection Molding

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.49 g/ccISO 1183
Water Absorption 0.20 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 0.80 %ISO 62
Maximum Moisture Content 0.15
Linear Mold Shrinkage, Flow 0.017 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.019 cm/cmISO 294-4
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 9140 psiISO 527-2
Elongation at Yield 9.5 %ISO 527-2
Tensile Modulus 551000 psiISO 527-1
Charpy Impact Unnotched 43.0 ft-lb/in²
@Temperature -30.0 °C
ISO 179
 43.0 ft-lb/in²
@Temperature 22.8 °C
ISO 179
Charpy Impact, Notched 1.70 ft-lb/in²
@Temperature -30.0 °C
ISO 179
 1.70 ft-lb/in²
@Temperature 22.8 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Constant 3.8
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 2200 V/milIEC 60243-1
Dissipation Factor 0.0060
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 44.0 µin/in-°FISO 11359-2
Melting Point 331 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 239 °FUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Melt Temperature 374 - 446 °F
Mold Temperature 140 - 248 °F
Drying Temperature 176 - 230 °F
Dry Time 2.00 - 4.00 hour
Injection Pressure 508 - 2470 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASG2131 / 310824

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.