MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Synfoam® UL-6 Syntactic Foam
Categories: Polymer; Thermoset

Material Notes: Pre-cast. SynFoam UL is a 100% closed cell, low density foam with exceptional compressive and insulation properties. UL grade foams are rigid, easily machined and can be sanded to a smooth finish. SynFoam UL is used for structural weight reduction, thermal insulation and as a replacement for honeycomb structures in aerospace applications. SynFoam is also used in the marine industry when a protective coating is applied to prevent water ingress. SynFoam UL is an ideal structural core material and has been used to replace honeycombs, PU and PVC based foams. SynFoam UL is chemically stable, UV resistant and does not absorb water. SynFoam UL is available as 6” x 12” x 24” fully cured blocks. The blocks may be further machined into different sizes and shapes by the end user to meet the necessary specific tolerances and requirements. Our syntactic foam is easily bonded together with the use of our syntactic adhesive to form large structures.

Information provided by Synfoam®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.00 - 8.00 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 50.0 psi
Compressive Modulus 2000 psi
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 1.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trelleborg AEM Syntac® 350 Syntactic Foam
Synfoam® SW-5 Syntactic Foam
Synfoam® SG-40 Syntactic Foam
Mitsubishi Chemical Advanced Materials Nylacel Low K Lower Thermal Conductivity Nylon-based Syntactic Foam, cast (ASTM Data)

PSYNF026 / 192901

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.