MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Eastman EEH Solvent
Categories: Fluid; Solvent

Material Notes: CAS No. 1559-35-9

Product Description: Eastman™ EEH Solvent (Ethylene Glycol 2-Ethylhexyl Ether) is primarily used in performance specialty coatings applications. It offers an excellent balance of performance properties when used as a coalescent in architectural and industrial maintenance coatings. Eastman™ EEH Solvent has low water miscibility, low surface tension, good hydrolytic stability, and high electrical resistance. In electrodeposition primers, Eastman™ EEH Solvent reduces volatilization from dip tanks and provides good flow and leveling of the coating in the baking oven. It is not a HAP or listed on SARA 313.

Application/Uses:

  • Coatings - Architectural
  • Coatings - Automotive OEM
  • Coatings - Automotive Refinish
  • Coatings - Can and Coil
  • Coatings - Consumer Electronics
  • Coatings - Floor Polishes
  • Coatings - General Industrial
  • Coatings - Industrial Maintenance and Marine
  • Coatings - Industrial Wood
  • Coatings - Transportation
Key Attributes:
  • Efficient coalescent
  • Low surface tension
  • Low water solubility
  • LVP-VOC
  • Non-HAP
  • Non-SARA
  • REACH compliant
  • Readily biodegradable
  • Slow evaporation rate

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.892 g/cc
Viscosity 7.0 cPLiquid
Vapor Pressure 0.0000296 atm
@Temperature 20.0 °C
 0.000590 atm
@Temperature 55.0 °C
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.010
 
Thermal PropertiesOriginal ValueComments
CTE, linear 93.0 µm/m-°C
Melting Point <= -100 °CFreezing Point
Boiling Point 226 °C@ 760 mm Hg, Initial
 275 °C@ 760 mm Hg, Dry Point
Flash Point 106 °CSetaflash Closed Cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.437
 
Descriptive Properties
ColorPt-Co

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5225 / 222419

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.