MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Keysor-Century KC1220 Rigid PVC Extrusion Blow Molding Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded

Material Notes: A general purpose extrusion blow molding compound for pine oil applications. KC1220 has an excellent balance of properties, offering outstanding clarity and gloss, high impact strength, and good color retention. Its excellent dynamic thermal stability enables easy processability with a wide variety of equipment and conditions. This permits extended production runs with minimum maintenance and downtime, and maximum regrind recycling. It is available in glass clear, and with various levels of blue tint as free flowing pellets.

KC1220 is recommended for use in a wide variety of packages for non-food applications, including pine oils. Suitable for simple Boston Round design or complex shapes and sizes for cosmetics, cleaning fluids, floor waxes, shampoos, detergents, bleaches, and engine oil.

Property values are typical values. Information provided by Keysor-Century Corporation.

Keysor-Century Corporation is no longer in business.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80ASTM D2240
Tensile Strength, Yield 45.0 MPaASTM D638
Modulus of Elasticity 2.34 GPaASTM D638
Flexural Yield Strength 72.0 MPaASTM D790
Flexural Modulus 2.48 GPaASTM D790
Izod Impact, Notched 9.60 J/cm
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %Available clear but manufacturer does not quantify.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Phosphorus deoxidized Copper high residual phosphorus, UNS C12200
Global PC/ABS-MC1220 General Purpose Polycarbonate/ABS Alloy

PKCV13 / 48706

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.