System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Multibase Multi-Pro® 1010 T Black 10% Talc Content Polypropylene
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene with 10% Talc Filler
Material Notes:
PPH talc filled compound suitable for containers and wash-tubs requiring elevated stiffness and improved cycle times.
Data provided by Multibase.
Key Words:
PP
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.974
g/cc
ASTM D792-91
Melt Flow
11
g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties
Original Value
Comments
Tensile Strength, Ultimate
33.8
MPa
ASTM D638-95
Elongation at Break
60 %
ASTM D638-95
Flexural Strength
46.9
MPa
ASTM D790-92
Flexural Modulus
2.00
GPa
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched
0.480
J/cm
ASTM D256-93a
Gardner Impact
0.700
J
ASTM D5420-93
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Multibase Multibatch® ME 50024 Sheet Extrusion
Multibase Multibatch® ME 50003 Anti-blocking Masterbatch
Multibase Multi-Pro® 4006 T H BLK 40% Talc Content Polypropylene
Multibase Multibatch® MP 52577 Sheet Extrusion
Multibase Multibatch® MP 52206 Sheet Extrusion
PLA249 / 49646
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.