MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
CBS-600 Carburizing Bearing and Gear Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; High Carbon Steel

Material Notes: CBS-600 VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F.

Information provided by Latrobe and the reference(s).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.282 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 41core layer, 0.20% C; oil-quenched from 1095°C (2000°F)
 62case layer, 0.7 to 1.0% C; oil-quenched from 1095°C (2000°F)
Tensile Strength, Ultimate 220 ksi24°C Test Temp
Tensile Strength, Yield 1250 MPa
@Strain 0.2 %
24°C Test Temp; 927°C Hardening Temp
 1265 MPa
@Strain 0.2 %
24°C Test Temp; 843°C Hardening Temp
 965 MPa
@Strain 0.2 %,
Temperature 371 °C
843°C Hardening Temp
 1020 MPa
@Strain 0.2 %,
Temperature 371 °C
927°C Hardening Temp
Elongation at Break 11.4 %24°C Test Temp; 843°C Hardening Temp
 12.5 %24°C Test Temp; 927°C Hardening Temp
 17.5 %
@Temperature 371 °C
843°C Hardening Temp
 18.2 %
@Temperature 371 °C
927°C Hardening Temp
Reduction of Area 43.5 %after 843°C Hardening Temp
 54.9 %after 927°C Hardening Temp
 53.6 %
@Temperature 371 °C
Modulus of Elasticity 30500 ksi
 24900 ksi
@Temperature 550.0 °C
Poissons Ratio 0.292
@Temperature 20.0 °C
 0.309
@Temperature 550.0 °C
Fracture Toughness 42.0 - 52.0 ksi-in½cracks originating in case; case depth 0.30 to 0.35 in.
 74.0 - 91.0 ksi-in½cracks originating in core
Shear Modulus 9300 ksi
@Temperature 538 °C
 11850 ksi
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.7 µm/m-°C
@Temperature 21.0 - 204 °C
0.20%C
 12.8 µm/m-°C
@Temperature 21.0 - 427 °C
0.20%C
Specific Heat Capacity 0.118 BTU/lb-°F
@Temperature 20.0 °C
 0.166 BTU/lb-°F
@Temperature 550.0 °C
Thermal Conductivity 33.9 W/m-K
@Temperature 550.0 °C
 48.6 W/m-K
@Temperature 20.0 °C
Maximum Service Temperature, Air 600 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 729 °CCritical Temperature Case Ac1
 729 °CCritical Temperature Core Ac1
 802 °CCritical Temperature Case Ac3
 885 °CCritical Temperature Core Ac3
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.060 %
Carbon, C 0.19 %
Chromium, Cr 1.45 %
Iron, Fe 95.6 %
Manganese, Mn 0.60 %
Molybdenum, Mo 1.0 %
Silicon, Si 1.1 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CBS-1000M High Temperature Bearing Steel
M50-NiL High Performance Carburizing Bearing and Gear Steel
AISI 4140 Steel, oil quenched, 205°C (400°F) temper, 25 mm (1 in.) round
AISI 6145 Steel (UNS G61450)
AISI 8740 Steel, normalized 870°C (1600°F)

MQZ9942 / 172239

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.