MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polynt S 320 LS Putty
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: S 320 LS “Blue Lightening” is a polyester resin based machineable putty. Blue lightening is intended for the fabrication of pattern facing with CNC routing or milling. When applied to a substructure this product provides a machineable, stable pattern surface for the creation of molds and prototypes. Blue lightening cuts into shavings, creates little or no dust, is sandable, repairable and compatible with most surface finishes. When used with MEKP catalysts containing a disappearing red color Blue lightening starts off a light mauve color to indicate the presence of catalyst and proper mixing. Upon gel the material fades to a light blue color.

Features And Benefits:

  • Pumps with standard polyester putty equipment from 5 or 45 gallon systems
  • Up to 30% higher yields over sprayed systems, 50% less labor intensive
  • Applies in a uniform thickness horizontally or vertically without sagging
  • Non porous surface, suitable for vacuum bagging
  • Machineable, repairable, easy to sand, easy on cutting tools
  • Low shrinkage
  • May be applied ¾” thick in one application
  • Machineable in under 24 hours, low wear on tools
  • Available in 20 liter pails and 200 liter drums

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.650 - 0.750 g/cc
Brookfield Viscosity 200000 - 250000 cPT-D @ 10rpm
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 70.0 °C
 
Processing PropertiesOriginal ValueComments
Gel Time 40.0 - 60.0 min1% MEKP 9 (United Initiators)
Shelf Life 1.50 Month
 
Descriptive Properties
Thixotropic Index>6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYN9021 / 231616

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.