MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Colmant Coated Fabrics Nitrile (NBR) Coated Cotton Fabric
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: The nitrile coated cotton fabric combines the following properties: Nitrile rubber has excellent resistance to petroleum products, fuels, aliphatic solvents, animal and vegetable oils and fats. Good resistance to polar or aromatic solvents. Good mechanical characteristics.
Limitations: It is highly flammable. It has a low resistance to cold, aging, sunlight, weather and ozone. Cotton is a natural fiber of vegetable origin. The cotton thread comes from the transformation of the hairs of the Gossypium (or cotton tree). We also designate under the same name the fabric resulting from the weaving of this thread. Cotton is the first textile fiber used in the world despite the advent of synthetic fibers. Flammable. It decomposes around 160°C. Cotton is popular thanks to its characteristics: appearance, lightness, comfort and ease of assembly and transformation.

Applications:

  • Industrial fabrics
  • straps
  • tarps
  • tires
  • rope
  • clothing
  • Gas tanks
  • The family AROMER
Properties:
  • Fireproofed
  • Non-skid
  • Oil storage
  • Fuel storage
  • Ozone Resistance
  • Cold resistance

Information provided by COLMANT COATED FABRICS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30 - 90
Tensile Strength at Break 8.00 - 20.0 MPa
Elongation at Break 100 - 900 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 115 °C
Minimum Service Temperature, Air -20.0 °C
 
Descriptive Properties
IRHD Hardness30-90
Point Temperature-20 C° - 120°C
Warp breaking strength75 - 120 daN/5cm
Warp elongation at break10% - 20%
Weft breaking strength70 - 90 daN/5cm
Weft elongation at break10% - 20%
Weight per sqm200 - 400

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOLMANT076 / 316126

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.