MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Borealis Borcoat™ BB700E-7032 Polypropylene Compound for Steel Pipe Coating Applications
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Borcoat BB700E-7032 is a grey colored high impact polypropylene. This product is especially designed for direct extrusion of syntactic PP with high thermal insulations capacity and high compression strength.

Borcoat BB700E-7032 is recommended as thermal insulation for offshore deep water flow lines.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183
Melt Flow 1.6 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63ISO 868
Tensile Strength, Yield 25.0 MPaAt 50 mm/min; ISO 527-2
Elongation at Break <= 200 %50 mm/min; ISO 527-3
Tensile Modulus 1.40 GPaAt 1 mm/min; ISO 178
Flexural Modulus 0.800 GPaAt 2 mm/min; ISO 178
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 145 °CA (10 N); ISO 306
 
Processing PropertiesOriginal ValueComments
Front Barrel Temperature 220 - 240 °C
Melt Temperature 225 - 235 °C
Head Temperature 220 - 230 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tipco Tipcolene® PP FR V0 - UL94-V0 Flame Retardant Polypropylene Homopolymer
Cossa Polimeri ESTAPROP 1050 V0 HF H Flame Retardant Polypropylene
Cossa Polimeri ESTAPROP 1040 V2 H Flame Retardant Polypropylene
Cossa Polimeri ESTAPROP 1000 V2 H Flame Retardant Polypropylene
Borealis BE60-7032 Grey Polypropylene Homopolymer for Pressure Pipes, Fittings and Sheets

PBOREA045 / 27352

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.