MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Zeus EFEP Tubing
Categories: Polymer; Thermoplastic; Fluoropolymer

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.74 g/ccASTM D792
Water Absorption <= 0.10 %ASTM D257
Crystallinity 10 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75ASTM D2240
Tensile Strength, Ultimate 40.0 - 50.0 MPaASTM D638
Elongation at Break 420 - 460 %ASTM D638
Modulus of Elasticity 0.490 - 0.780 GPaASTM D638
Flexural Modulus 0.880 - 1.37 GPaASTM D790
Coefficient of Friction 0.055 - 0.078
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.6
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 400 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 - 90.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Thermal Conductivity 0.240 W/m-KASTM C177
Melting Point 160 - 195 °C
Maximum Service Temperature, Air 150 °C
Decomposition Temperature 350 °CASTM E1131
Oxygen Index 31 %ASTM D2863
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.338 - 1.34

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Daikin NEOFLON® RP-5000AS Tubing Grade EFEP
Daikin NEOFLON® RP-4040 EFEP Pellets
Syensqo (Solvay Specialty Polymers) Halar® 500 ECTFE Fluoropolymer
Syensqo (Solvay Specialty Polymers) Halar® 3404DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE), Filled
Syensqo (Solvay Specialty Polymers) Halar® 300 ECTFE Fluoropolymer

PZEUS996 / 178061

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.