MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DIAB Klegecell® R 45 Rigid, Closed Cell PVC Foam Core Material  (discontinued **)
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoplastic; Vinyl (PVC); PVC, Foam Grade

Material Notes: Klegecell R is a PVC based, rigid, closed-cell foam with a tri-dimensional grid structure, which provides high thermal stability and structural integrity. As a structural core, Klegecell R is used in conjunction with high strength facings to produce lightweight, yet exceptionally stiff composite structures. Klegecell is widely used and found in pleasure crafts, tanks, high performance boats, vehicles, and many other high-strength, low-weight applications.

Information provided by DIAB, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.80 lb/ft³Nominal
 2.52 - 3.22 lb/ft³Tolerance from nominal of -10%/+15%.; ISO 845
Water Vapor Transmission 7.50 g/m²/dayISO 1663
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 131 psiISO 1926
Elongation at Break 10 %Shear Strain
Tensile Modulus 0.0320 GPa
Compressive Strength 73.0 psiISO 844
Compressive Modulus 8700 psiASTM D1621-B
Poissons Ratio 0.32
Shear Modulus 2.755 ksiISO 1922
Shear Strength 87.0 psiISO 1922
 
Thermal PropertiesOriginal ValueComments
CTE, linear 35.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Specific Heat Capacity 0.454 BTU/lb-°F
Thermal Conductivity 0.0230 W/m-K
@Temperature 10.0 °C
ASTM C518
Insulation R Value 3.20.5 inch sample; based on a +10°C K factor.
 6.31.0 inch sample; based on a +10°C K factor.
 12.62.0 inch sample; based on a +10°C K factor.
Maximum Service Temperature, Air 70.0 °CContinuous
Minimum Service Temperature, Air -200 °CContinuous
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 80.0 °C
 
Descriptive Properties
Water Absorption0.021 lb/ft²ASTM C272

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DIAB Klegecell® R 60 Rigid, Closed Cell PVC Foam Core Material
Overview of materials for PVC, Foam Grade
CoreLite Board® Closed-Cell PVC Foam
CoreLite PVC 48 Closed-Cell PVC Foam Sheet
DIAB Klegecell® R 260 Rigid, Closed Cell PVC Foam Core Material

PDIAB24 / 29816

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.