MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Phillips 66 Multiplex® Red NGLI Grade 1
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Multiplex Red is a high-performance, multipurpose, extreme pressure (EP) lithium complex grease developed for the lubrication of automotive and industrial equipment operating under heavy loads and at moderate to high temperatures. It is particularly recommended for use in applications that are too severe or require higher performance than that provided by conventional extreme-pressure lithium greases. Multiplex Red is manufactured with high-quality base oils and a lithium complex soap thickener. It is fortified with extreme pressure and antiwear additives, a tackifier, and rust and oxidation inhibitors to provide outstanding wear protection, excellent thermal stability at high temperatures, and excellent resistance to corrosion and water washout. It forms an effective seal to help minimize bearing contamination and provides a high level of adhesion to bearing surfaces for improved retention, reduced leakage and excellent resistance to water washout. It is dyed red for ease of identification. Multiplex Red Grades No. 1 and No. 2 are NLGI GC-LB certified for use as multipurpose automotive wheel bearing and chassis lubricants.

Applications:

  • Wheel bearings of passenger cars, trucks, high-performance vehicles, sport utility vehicles and motorcycles, particularly vehicles equipped with disc brakes
  • Ball joints, universal joints, other chassis parts and water pumps on passenger cars, trucks and other mobile equipment
  • Heavily loaded plain and rolling element bearings in industrial, mining and mobile equipment
Features/Benefit:
  • Excellent high-temperature performance
  • Outstanding wear protection
  • High load-carrying capacity
  • Protects against rust and corrosion
  • Good low-temperature pumpability
  • NLGI GC-LB certified (Grades No. 1 and No. 2)

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.48 lb/gal
Viscosity Measurement 70Index
Saybolt Viscosity at 100°F 905 SUS
Saybolt Viscosity at 210°F 75 SUS
Kinematic Viscosity at 40°C (104°F) 170 cSt
Kinematic Viscosity at 100°C (212°F) 13.8 cSt
Oxidative Stability 100 hour
@Pressure 0.0345 MPa
Pressure Drop; ASTM D942
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 400 kgASTM D2596
Four Ball Wear <= 0.600 mmScar Diameter; ASTM D2266
Penetration 310 - 340
Timken Test 70.0 lbOK Load; ASTM D2509
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 177 °C
Minimum Service Temperature, Air -34.0 °C
Dropping Point 271 °C
 
Descriptive Properties
ColorDark Red
ThickenerLithium Complex
US Steel Mobility0.11 g/sec-18°C
 0.57 g/sec-7°C
 2.18 g/sec4°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5128 / 198381

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.