MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound LCL33 Polyetheretherketone (PEEK) (Americas)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: LNP LUBRICOMP LCL33 compound is based on Polyetheretherketone (PEEK) resin containing 15% carbon fiber, 15% PTFE. Added features of this grade include: Wear Resistant, Electrically Conductive.

Features: Light-weight Structural,Super Strong (Carbon Fiber Filled),Wear resistant,Electrically Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.43 g/ccASTM D792
 1.43 g/ccISO 1183
Moisture Absorption 0.0700 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm24hrs; ASTM D955
 0.0010 - 0.0030 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0030 - 0.0070 cm/cm24hrs; ISO 294
 0.0040 - 0.0070 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 179 MPaASTM D638
 187 MPaISO 527
Elongation at Break 1.6 %ISO 527
 1.7 %ASTM D638
Tensile Modulus 14500 MPa1 mm/min; ISO 527
 16610 MPa50 mm/min; ASTM D638
Flexural Strength 230 MPaISO 178
 262 MPaASTM D790
Flexural Modulus 11700 MPaISO 178
 12960 MPaASTM D790
Izod Impact Notched 64.0 JASTM D256
Izod Impact, Unnotched 480 J/mASTM D4812
Izod Impact, Notched (ISO) 7.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 34.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 9.00 Jpeak; ASTM D3763
Impact Test 9.00 JMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.35ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.28ASTM D3702 Modified: Manual
K (wear) Factor 17.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 23.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 23.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 41.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 41.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) >= 300 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 >= 298 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 380 - 400 °C
Zone 3 380 - 400 °C
Mold Temperature 175 - 190 °C
Drying Temperature 150 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa
Screw Speed 60 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80871 / 288818

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.