OREVAC PPC is a grafted maleic anhydride polypropylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC PPC is mainly used in multi-layer tube to have good adhesion between PP, PA and EVOH. OREVAC PPC combined with SOARNOL®from NIPPON GOSHEI provides very good oxygen barrier. These tubes are used in plumbing, sanitary, heating floor and also industrial applications.Information provided by Arkema Group |