ELASTOSIL® R 510/60 is a peroxide curing HTV silicone rubber, which is exclusively intended for the manufacture of silicone-insulated cables. Special features: - good mechanical properties
- good heat resistance
- good rheological properties
Application: Cables in general.Information provided by Wacker Chemie AG. |