MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shandong Dawn Dawnprene 810-45D TPV (EPDM/PP)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Uses: Automotive - Exterior Parts: scuff strip

Information provided by Shandong Dawn Polymer Material Co.,Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.945 g/ccISO 1183
Linear Mold Shrinkage 0.0080 - 0.013 cm/cmISO 294
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
GB/T3682
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 45ISO 7619
Tensile Strength 15.5 MPaISO 37
Elongation at Break 580 %ISO 37
Izod Impact, Notched (ISO) 12.0 kJ/m²
@Temperature -30.0 °C
ISO 180
 NB
@Temperature 23.0 °C
ISO 180
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 56.0 °CISO 75
 
Descriptive Properties
Accelerated Weathering SAE J25271.9Delta E, 2500KJ
Elongation Change (%) ISO 188-20.8change @ heat aging 100°C, 1000hr
Tensile Change (%) ISO 188-15.6change @ heat aging 100°C, 1000hr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polykemi AB POLYelast TPE EC90 D50 P05B Thermoplastic Elastomer, PP/EPDM
Shandong Dawn Dawnprene 11-40D TPV (EPDM/PP)
Shandong Dawn Dawnprene 14-50A TPV (EPDM/PP)
Shandong Dawn Dawnprene D-85A TPV (EPDM/PP)
Polykemi AB POLYfill PP EVR8025H UV Polypropylene/EDPM, Mineral Reinforced

PSHAND950 / 192586

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.