MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Sandvik Sanicro 28 Precision Wire
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: Sanicro 28 is a high ­alloy austenitic stainless steel suitable for service in highly corrosive oil and gas environments. The grade is characterized by:
  • Very good corrosion resistance in H2S, CO2 and chloride containing environments.
  • Very good resistance to pitting owing to its high PRE* value of 38 minimum
  • General corrosion comparable to or better than Alloy 825
  • Tensile strength equivalent to ASTM 316
  • Very good performance in elevated temperatures (geothermal wells)
  • Entirely non-magnetic properties
Information provided by Sandvik

Key Words: UNS N08028
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/ccBased on UNS number
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 1500 MPa
Tensile Strength, Yield >= 1350 MPa
@Strain 0.2 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.020 %
Chromium, Cr 27 %
Copper, Cu 1.0 %
Iron, Fe 34.8 %As Balance
Manganese, Mn 2.0 %
Molybdenum, Mo 3.5 %
Nickel, Ni 31 %
Phosphorus, P <= 0.025 %
Silicon, Si 0.60 %
Sulfur, S <= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals INCOLOY® alloy 028 Austenitic Stainless Steel
Industeel URANUS® B28 High Nickel Super-Austenitic Stainless Steel

NSANDV218 / 19112

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.