MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Aperam Superimphy® 600 Bar-Corrosion application
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: It is a Ni Cr Fe alloy with good oxidation resistance at high temperatures and corrosion resistance to chloride ion stress-corrosion cracking. It also has a good caustic corrosion resistance. It is a non-magnetic alloy.

Applications:

  • Chemical Industries and food
  • Furnace components
  • Nuclear industry
  • Automotive (spark plug)
Standards related to these applications: ASTM B166 or B564; NACE MR0175; AMS 5687 or 5665

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 14 - 17 %
Iron, Fe 6.0 - 10 %
Nickel, Ni 73 - 80 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
H.C. Starck Amperit® 335.066 Nickel Self-fluxing Alloy HRC 60 (NiCrBSi)
MetalTek MTEK CY-40 Cast UNS N06040 Severe Corrosion and Heat Resistant Alloy
Illium W Cast Nickel Superalloy
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750)
H.C. Starck Amperit® 119.075 Molybdenum-Nickel SF RC 60 75-25 (Mo / NiSF)

NPERA024 / 194813

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.