MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Selenis WEEZEN HS 410 Copolyester for Shrink Sleeves
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Selenis Weezen HS 410 is a copolyester specifically developed for full body shrink sleeves, a packaging solution that will make products stand out on the shelf. These full-body labels maximize marketing space as they allow 360º printing of eye-catching graphics with excellent printability, clarity and gloss. The Selenis Weezen HS 410 is the copolyester solution that will enhance brand image and increase consumer brand loyalty. Selenis Weezen HS 410 is the ideal solution for any kind of packaging: beverage, soft drinks, juices, alcoholic drinks, personal care, household products, and labels to fit high contour containers. Labels made with Selenis Weezen HS 410 copolyester will shrink perfectly around any shape when heat is applied. Full-body shrink sleeve labels made from Selenis Weezen HS 410 allow tamper-evident packaging, promoting a sense of security to customers whilst reducing packaging cost as there is no need for plastic rings or other tamper evident bands. The portion of the sleeve covering the cap can be perforated to make it easier for the customer to open. Selenis Weezen HS 410 maintains excellent transparency and clarity even after long exposure to temperatures higher than its glass transition temperature (Tg) given the product’s tendency not to crystallize.

Information provided by Selenis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.730 g/cc
Density >= 1.27 g/ccASTM D792
Viscosity Test 76 - 80 cm³/gIntrinsic; ISO 1628-5
ASTM Color <= 1.0b*; ASTM D6290
 >= 64L*; ASTM D6290
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 50.0 MPa(σm); ISO 527 -1/- 2
Tensile Strength, Yield 50.0 MPa(σy); ISO 527 -1/- 2
Elongation at Break 84 %Nominal, (εtb); ISO 527 -1/- 2
Elongation at Yield 4.2 %(εm); ISO 527 -1/- 2
 4.2 %(εy); ISO 527 -1/- 2
Flexural Strength 61.0 MPaISO 178
Flexural Modulus 1822 MPaISO 178
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 81.9 °CISO 306/A50
Glass Transition Temp, Tg 85.0 °CASTM D3418
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 250 °C
Drying Temperature <= 70.0 °Cto avoid chips sticking together in dryer hopper
 65.0 °C
@Time 21600 - 28800 sec
Moisture Content <= 0.0040 %dried
Dew Point -40.0 °C
 
Descriptive Properties
Particle size320 ± 50 mg/20 chips
Pellet ShapeCylindrical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSELE910 / 243408

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.