Product highlights: CABELEC CA6497 conductive compound is an electrically conductive compound made from a carefully selected carbon black finely dispersed in high density polyethylene (HDPE) resin. Its electrical and mechanical properties are not dependent on atmospheric conditions. It has been developed for injection molding applications. This product is suitable for use in a wide range of plastics that come into contact with food in North America region. For more details regarding the status against the FDA legislation, please contact your usual Cabot representative.Information provided by Cabot Corporation |