MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Daikin POLYFLON D-1E PTFE Dispersion
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: POLYFLON PTFE aqueous dispersions are normally stabilized with non-ionic surfactants and contain 60% POLYFLON PTFE by weight.

Processing Methods: Impregnation, casting, coating.

Applications: Anti-stick coating, packings, cast film.

Information provided by Daikin Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.52 g/cc
@Temperature 25.0 °C
Particle Size 0.20 - 0.40 µm
pH 9.0 - 10
Viscosity 25 cP
@Temperature 25.0 °C
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 1.9 - 2.1
@Frequency 1000 Hz
PTFE Component; ASTM D150
 1.9 - 2.1
@Frequency 1e+6 Hz
PTFE Component; ASTM D150
Dissipation Factor 0.00010 - 0.00022PTFE Component
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0PTFE Component
Oxygen Index >= 95 %PTFE Component

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Teflon® PTFE Grade 30 Aqueous Dispersion
3M Dyneon™ TF 5070GZ PTFE Dispersion
3M Dyneon™ TF 5033Z PTFE Dispersion
Chemours Teflon® PTFE Grade 305A Aqueous Dispersion
Daikin PTFE D-210 DISPERSION Polytetrafluoroethylene Aqueous Dispersion

PDAIK027 / 29319

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.