Novolac resin based, glass fiber and glass beads reinforced. Very easy to transform in complex shapes. Excellent mechanical and thermal properties. Higher isotropic properties and good dimensional stability. Specially used in Powertrain SystemsInformation provided by Sumitomo Bakelite North America, Inc. |