MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cossa Polimeri ESTAPROP 1050 V0 HF H Flame Retardant Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: PP homopolymer

Flame retardant class V0, halogen free, excellent mechanical characteristics, excellent processability

Information provided by Cossa Polimeri S.r.l.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccASTM D 792
Linear Mold Shrinkage 0.012 - 0.015 cm/cmASTM D 955
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 25.0 MPaASTM D 638
Elongation at Break 20 %ASTM D 638
Flexural Modulus 2200 MPaASTM D 790
Izod Impact, Notched 20.0 J/m
@Temperature 0.000 °C
ASTM D 638
 25.0 J/m
@Temperature 23.0 °C
ASTM D 256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C120°C/hr; ASTM D 648
Vicat Softening Point 155 °C
@Load 0.999 kg
50°C/hr; ASTM D 1525
Flammability, UL94 V-0
@Thickness 1.60 mm
 V-0
@Thickness 3.20 mm
Glow Wire Test 960 °C
@Thickness 2.00 mm
I.E.C. 695-2-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tipco Tipcolene® PP FR V0 - UL94-V0 Flame Retardant Polypropylene Homopolymer
Cossa Polimeri ESTAPROP 1000 V2 H Flame Retardant Polypropylene
Cossa Polimeri ESTAPROP 1040 V2 H Flame Retardant Polypropylene
Avient Maxxam® DP-7032-1 20% Calcium Carbonate Reinforced Polypropylene, LTHA
Borealis Borcoat™ BB700E-7032 Polypropylene Compound for Steel Pipe Coating Applications

PCOSSA880 / 156470

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.