DOWLEX® 2037 Polyethylene is a cast film extrusion resin for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a when used unmodified and according to good manufacturing practices for food contact applications. The regulation should be consulted for complete details. Film properties below based on a film thickness of 30 µm. Data provided by Dow Chemical. |