Good to excellent corrosion resistance. Excellent machinability, good cold workability. Fabricated by blanking, drawing, bending, machining, shearing, stamping. Applications: bearings, bushings, gears, pinions, shafts, thrust washers, valve parts. Test specimen: flat products - 8mm thickness. |