MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Celanese Zytel® (PA66) 70G30HSLR BK186LM PA66-GF30
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: 30% Glass Reinforced, Heat Stabilized, Hydrolysis Resistant,  Laser Markable  Polyamide 66

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccDAM; ISO 1183
Melt Density 1.20 g/cc
@Temperature 295 °C
Viscosity Number 150 cm³/gDAM; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0030 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 130 MPa50% RH; ISO 527-1/-2
 190 MPaDAM; ISO 527-1/-2
Elongation at Break 3.0 %DAM; ISO 527-1/-2
 5.0 %50% RH; ISO 527-1/-2
Tensile Modulus 7000 MPa50% RH; ISO 527-1/-2
 10000 MPaDAM; ISO 527-1/-2
Flexural Strength 200 MPa50% RH; ISO 178
 280 MPaDAM; ISO 178
Flexural Modulus 6500 MPa50% RH; ISO 178
 9000 MPaDAM; ISO 178
Poissons Ratio 0.34DAM
 0.3550% RH
Izod Impact, Notched (ISO) 10.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 12.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 65.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 80.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 10.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 12.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 400 VDAM; IEC 60112
Hot Wire Ignition, HWI 7.0 sec
@Thickness 0.750 mm
DAM; UL 746A
 7.0 sec
@Thickness 1.50 mm
DAM; UL 746A
 60 sec
@Thickness 3.00 mm
DAM; UL 746A
High Amp Arc Ignition, HAI 120 arcs
@Thickness 0.750 mm
DAM; UL 746A
 120 arcs
@Thickness 1.50 mm
DAM; UL 746A
 120 arcs
@Thickness 3.00 mm
DAM; UL 746A
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 2.22 J/g-°C
@Temperature 295 °C
Melt
Thermal Conductivity 0.220 W/m-K
@Temperature 295 °C
Melt
Melting Point 262 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 253 °CDAM; ISO 75-1/-2
Glass Transition Temp, Tg 20.0 °C10°C/min; 50% RH; ISO 11357-1/-2
 75.0 °C10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 0.750 mm
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
Oxygen Index 24 %DAM; ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 295 °COptimum, Injection
 285 - 305 °CRange, Injection
Mold Temperature 70.0 - 120 °CInjection
 100 °COptimum, Injection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %Injection
Hold Pressure 50.0 - 100 MPaRange, Injection
 
Descriptive Properties
AdditivesRelease agent
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA66,GF30,M1CGHO2RW,S14-100
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PA66-GF30<ISO 11469
PolymerPA66-GF30
Processing Hold Pressure Time (s/mm)3Injection
Resin IdentificationPA66-GF30ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSX5325b / 254526

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.