Availability: North America Forms: Pellets Filler/Reinforcement: Glass Bead, 10% Filler by Weight and Glass Fiber Reinforcement, 20% Filler by Weight Additive: Lubricant and Heat Stabilizer Features: Lubricated and Heat Stabilized Information provided by TP Composites, Inc. |