Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive instrument panels in which good surface finish, high scratch resistance and good UV resistance are required. Availability: Africa & Middle East and Europe Features: - Balanced Stiffness/Toughness
- Good Surface Finish
- High Impact Resistance
- High Scratch Resistance
- Low to No Fogging
Uses: - Automotive Applications
- Automotive Instrument Panel
- Automotive Interior Parts
- Automotive Interior Trim
Processing Method: Injection MoldingInformation provided by ExxonMobil |