MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Colmant Coated Fabrics CSM (HYPALON®) Coated Aramid Tire Cord
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Tire cord fabric is a type of industrial fabric which is constructed using High Tenacity yarns in the warp direction and yarns of negligible resistance in weft direction which is used to hold warn yarns locked in their position. Tire cord coated fabrics provides fundamental properties such as controlled deformation, high strength, abrasion resistance, etc. Widely used by the tire industry, it is also employed for the rubber hose manufacture, air springs, expansion joints, among many other applications. Fiber consisting of a long chain polymer containing amines and aromatic components. Infusible, does not melt, does not burn, does not soften. Besides it shows low emission of toxic gases while combustion. Certain aramid can decompose at 500 ° C, It is thermostable up to 250 ° C. Chlorosulphonated Polyethylene or CSM – also known as Hypalon® – is to be considered an improved chloroprene as it offers better chemical resistance, ozone and light resistance, heat ageing. Their particular resistance to weathering conditions and the excellent low gas permeability presents CSM as the best option for the manufacture of premium quality inflatable boats and structures for all environments, but most of all in sea environment.

Applications:

  • Expansion joints
Properties:
  • Heat resistant
  • Fireproofed
  • Acids resistance
  • Non-skid
  • UV resistance
  • Water resistance
  • Ozone Resistance
  • Cold resistance

Information provided by COLMANT COATED FABRICS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30 - 90
Tensile Strength at Break 8.00 - 20.0 MPa
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °C
Minimum Service Temperature, Air -40.0 °C
 
Descriptive Properties
IRHD Hardness30-90
Point Temperature-40 C° - 130°C
Warp breaking strength350 - 5000 daN/5cm
Warp elongation at break2% - 5%
Weft breaking strength350 - 2000 daN/5cm
Weft elongation at break2% - 5%
Weight per sqm100 - 650

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOLMANT021 / 316071

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.