MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Chesterton 785 Parting Lubricant
Categories: Fluid; Lubricant

Material Notes: A proprietary blend of ultra-fine inorganic solid lubricants in a non-carbonizing, ashless synthetic carrier, 785 Parting Lubricant can be used under extremely severe conditions of temperature and pressure to assist in assembly and in assembly of threaded components. Chesterton 785 Parting Lubricant contains no toxic heavy metals. Plant personnel need not be concerned with health hazards associated with nickel or lead. Because 785 Parting Lubricant utilizes a synthetic con-carbonizing base, the product can be used over a broad temperature range. Hardening will not occur when used between -34°C to 1204°C (-30°F to 2200°F).

Features:

  • No Toxic Heavy Metals
  • For Extreme Pressure- up to 4730 kg/cm2 (67, 570 psi)
  • Broad Service Temperature Range
  • Ultra-Fine Particles
  • Balanced Coefficient of Friction
  • NSF H2 – Registration number 133960

Benefits:

  • Safer to workers
  • Usable under most extreme conditions
  • Will not carbonize
  • No need for torque tension recalculation
  • Fills in microscopic voids>Suggested Uses: Bolts, screws, studs, pipe threads, press fits, pump sleeves and splines. Use in power plants, textiles mills, bakeries, foundries, steel mills, boiler rooms, oil refineries, marine applications, chemical plants, automotive industry.

    Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/cc
Particle Size <= 25 µm
 
Mechanical PropertiesOriginal ValueComments
Coefficient of Friction, Dynamic 0.1040 kgf, 1200 rpm; ASTM D2266
Four Ball Extreme Pressure, Load Wear Index 67570[psi]; ASTM D2596, DIN 51 350
Four Ball Extreme Pressure, Weld Load 400 kgASTM D2596, DIN 51 350
Penetration 32.3[mm], Unworked; ASTM D217, ISO 2137
 33.4[mm], Worked; ASTM D217, ISO 2137
K Factor (Wear Factor) 0.17
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1204 °C
Minimum Service Temperature, Air -34.0 °C
Dropping Point >= 316 °CASTM D566, ISO2176
 
Descriptive Properties
ColorMetallic gray
ConsistencySoft Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sinotek Materials Tungsten Disulfide (WS2) Powder, High-Purity
DuBois Partherm 430 Heat Transfer Salt
DuBois Low Temperature Draw Salt Quenching and Tempering Salt
Chesterton 710 Anti-Seize Compound
Brandenburger Heavy Duty Mounting Paste

PPTCHS094 / 138206

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.