SR574 is a 10% mineral filled polypropylene compound intended for injection molding. Special Features: - Good flow
- Excellent stiffness and impact balance
Applications: SR574 has been developed especially for the car industry to be used in automotive exterior parts. Values determined on standard injection molded specimens conditioned at 23°C and 50% relative humidity after at least 96 hours storage time. To avoid residual humidity from transport or storage, the material should be pre-dried approximately 2h at 95° - 105°C.Information provided by Borealis AG |