MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Arkema Kynar Flex® 2850 WR PVDF
Material Notes:

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.77 - 1.80 g/ccASTM D792
Viscosity 400000 - 800000 cP
@Shear Rate 100 1/s,
Temperature 230 °C
Melt; ASTM D3835
Melt Flow 7.5 g/10 min
@Load 3.80 kg,
Temperature 230 °C
cm³/10 min Volumetric Rate; ISO 1133
 8.0 - 25 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70 - 75ASTM D2240
Tensile Strength at Break 27.6 - 48.3 MPaASTM D638
Tensile Strength, Yield 35.0 MPaDry; ISO 527-1/-2
 31.0 - 41.4 MPaASTM D638
Elongation at Break >= 50 %Dry; ISO 527-1/-2
 30 - 200 %ASTM D638
Elongation at Yield 5.0 - 15 %ASTM D638
 10 %Dry; ISO 527-1/-2
Tensile Modulus 1030 - 1520 MPaASTM D638
Flexural Strength 20.7 - 34.5 MPa
@Strain 5.0 %
ASTM D790
Flexural Modulus 1030 - 1240 MPaASTM D790
Compressive Strength 41.4 - 58.6 MPaASTM D695
Izod Impact, Notched 160 - 427 J/mASTM D256
Izod Impact, Unnotched NBASTM D256
Coefficient of Friction, Dynamic 0.19vs. steel; ASTM D1894
Coefficient of Friction, Static 0.25vs. steel; ASTM D1894
Taber Abrasion, mg/1000 Cycles 6.0 - 9.0CS 17 1000g:pad; ASTM-G195-13A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+14 ohm-cm65% R.H; ASTM D257
 2.00e+14 ohm-cmDry; IEC 60093
Dielectric Constant 3.5 - 10.2
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 1.30 - 1.60 kV/mmASTM D149
Dissipation Factor 0.010 - 0.22
@Frequency 100000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 126 - 185 µm/m-°CASTM D696
Specific Heat Capacity 0.745 - 0.958 J/g-°CDSC
Thermal Conductivity 0.144 - 0.180 W/m-KASTM D433
Melting Point 155 - 160 °CASTM D3418
 158 °C10°C/min; Dry; ISO 11357-1/-3
Maximum Service Temperature, Air 140 °CUL RTI
Deflection Temperature at 0.46 MPa (66 psi) 60.0 - 75.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °CDry; ISO 75-1/-2
 37.8 - 55.0 °CASTM D648
Glass Transition Temp, Tg -40.6 - -38.3 °CASTM D7028
Decomposition Temperature 375 °C1% wt. loss, TGA, in air
 410 °C1% wt. loss, TGA, in nitrogen
Flammability, UL94 V-0
@Thickness 0.800 mm
IEC 60695-11-10
Oxygen Index 43 %ASTM D2863
 43 %Dry; ISO 4589-1/-2
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.42sodium D line; ASTM D542
 
Descriptive Properties
Moisture SensitiveNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Kynar Flex® 3120-10 PVDF
Arkema Kynar® 705 PVDF
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
Arkema Kynar Flex® 3030-10 PVDF
Mitsubishi Chemical Advanced Materials Symalit® PVDF (ASTM Product Data Sheet)

PARKF707 / 193516

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.