MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Poly Alloy XuanWu™ XW7301 Modified Polyphenylenether
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Material Notes: XuanWu XW7301 resin is a modified polyphenylenether (mPPE) compound. XW7301 offers good performance on impact property, paintability, heat resistance, stiffness and chemical resistance.

Information provided by Poly Alloy Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.065 g/ccASTM D792
Melt Flow 8.0 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 450 kg(f)/cm²ASTM D638
Elongation at Break 60 %ASTM D638
Tensile Modulus 10000 kg(f)/cm²ASTM D638
Flexural Strength 9960 psiASTM D790
Flexural Modulus 18000 kg(f)/cm²ASTM D790
Izod Impact, Notched 10.0 kg-cm/cm
@Temperature -30.0 °C
ASTM D256
 24.0 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 186 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 280 °C
Middle Barrel Temperature 270 - 290 °C
Front Barrel Temperature 270 - 290 °C
Nozzle Temperature 270 - 290 °C
Mold Temperature 80.0 - 90.0 °C
Drying Temperature 120 °C
Dry Time 4.00 hour
Shelf Life 24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPALLOY112 / 278391

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.