MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
LyondellBasell Pro-fax 6329 Polypropylene Homopolymer, Improved Chemical Resistance
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:
Key Features: improved chemical resistance polypropylene homopolymer resin, FDA acceptable, easier processing

Applications: closures, housewares, chairs

Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.

Description: Pro-fax 6329 polypropylene homopolymer resin is designed for applications that require easier processing and improved chemical resistance properties. This resin is available in pelletized form. It meets FDA requirements in the Code of Federal Regulations in 21 FR 177.1520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792B
Melt Flow 14 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 30.0 MPaASTM D638
Elongation at Yield 12 %ASTM D638
Flexural Modulus, 1% Secant 1.20 GPa0.05 in/min; ASTM D790A
Izod Impact, Notched 0.300 J/cmASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °CASTM D648
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Pro-fax SV258 Polypropylene Impact Copolymer
Flint Hills P4G4Z-011 Homopolymer Polypropylene
Flint Hills P4C5Z-027 Homopolymer Polypropylene
Delrin Delrin® 100P BK602 POM
LyondellBasell Pro-fax PD702 Polypropylene Homopolymer, High Flow

PMO012 / 53493

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.