MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total Finathene® 3407B Black HDPE pipe grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe relining

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.958 g/ccASTM D 792
Environmental Stress Crack Resistance >= 1000 hourNo failures, compressed ring, 25% Igepal; ASTM F 1248
 >= 5000 hourNo failures; ASTM D 1693 cond. C
Carbon Black Loading 2.5 %ASTM D 1603
Melt Flow 0.38 g/10 min
@Load 5.00 kg
ASTM D 1238
High Load Melt Index 11 g/10 min
@Load 21.6 kg
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
PENT >= 400 hourASTM F 1473
Hardness, Shore D 63ASTM D 2240
Tensile Strength, Yield >= 3300 psiASTM D 638 type IV
Elongation at Break >= 800 %ASTM D 638 type IV
Flexural Modulus 125000 psiASTM D 790
Secant Modulus 0.793 GPa2% Strain; ASTM D 638 type IV
Izod Impact, Notched 8.00 ft-lb/in
@Thickness 3.17 mm
ASTM D256 A
Hydrostatic Design Basis 1600 psi
@Temperature 23.0 °C
ASTM D 2837
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 µin/in-°F
@Temperature 20.0 °C
ASTM D 696
Melting Point 258 °FASTM D3417
Deflection Temperature at 0.46 MPa (66 psi) 172 °FASTM D 648
Vicat Softening Point 255 °FASTM D 1525
Brittleness Temperature -118 °CASTM D 746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips HiD® 9300 HDPE Orange Pipe Resin
Chevron Phillips Marlex® HP076 High Density Polyethylene, Pipe Grade
Borealis BorSafe™ HE3494-LS-H HDPE Compound for Pressure Pipes
Borealis BorSafe™ HE3490-LS-H HDPE Compound for Pressure Pipes
Chevron Phillips Marlex® 9346 HDPE Natural Pipe Resin

PFINAP110 / 38693

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.