MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Ajedium™ Film Thermoplastic Polyimide
Categories: Polymer; Film; Thermoplastic; Polyimide, Thermoplastic

Material Notes: PI film, highest heat resistance, excellent chemical and radiation resistance

TPI is a thermoplastic polyimide film that has excellent, thermal, chemical, electrical and physical properties. With a continuous use temperature to 240°C (465°F), TPI films offer superior radiation resistance, excellent wear performance and resistance to chemicals.

Applications: Aircraft Applications; Automotive Applications; Electrical/Electronic Applications; Industrial Applications; Medical/Healthcare Applications; Oil/Gas Applications

Features: Chemical Resistant; Flame Retardant; Good Electrical Properties; High Heat Resistance; Radiation (Gamma) Resistant

Standard Thicknesses and Widths
- Widths are available from 22" (559 mm) to 56" (1422 mm). Products with widths <22 inches or >56 inches are available upon request.
- Tolerances for widths are +/- 4mm.
- For PI film, the standard thicknesses are 25 microns (1 mil) to 1016 microns (40 mil).

Surface Finishes
- Standard surface finish is P/M (polished / matte).
- Custom finishes of P/P (polished / polished) and M/M (matte / matte) are available.

Packaging
- Film is supplied in a roll form of high quality, cardboard core of 3" (76mm) or 6" (152mm).
- PVC cores are available upon request in 3" and 6" sizes.

Labeling
- Products are labeled to comply with national and international standards.
- Labels include product grade, unique batch number, roll length, roll width, product thickness, and net weight.

Information provided by Solvay Specialty Polymers.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.33 g/ccASTM D792
Water Absorption 1.0 %
@Time 86400 sec
ASTM D570
Thickness 100 micronsAs Tested
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 190 %ASTM D882
Film Elongation at Yield, MD 7.0 %ASTM D882
Secant Modulus, MD 3.05 GPaASTM D882
Dart Drop Test 400 gASTM D1709
Film Tensile Strength at Break, MD 104 MPaASTM D882
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmASTM D257
Dielectric Constant 2.5
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 160 kV/mm
@Thickness 0.100 mm
ASTM D149
Dissipation Factor 0.0014
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Melting Point 388 °CPeak; ASTM D3418
Glass Transition Temp, Tg 250 °CDSC
Oxygen Index 47 %ASTM D2863
 
Descriptive Properties
Area Factor145 ft²/lb/mil
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorOrange
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4008 / 279808

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.