MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Contact Metal, UNS C83300, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Sand.

Applications: Terminal ends for electrical cables.

Classified under: Red Brasses and leaded red brasses

Data typical for as-sand-cast separately cast test bars (M01 temper). Alloy does not respond to heat treating

Key Words: CA 833, contact metal, Ingot code no. 131
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 35500 kg, typical
Tensile Strength, Ultimate 220 MPa
Tensile Strength, Yield 70.0 MPa
@Strain 0.5 %
Elongation at Break 35 %In 50 mm
Modulus of Elasticity 105 GPa
Machinability 35 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000005388 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.380 J/g-°C
Melting Point 1030 - 1060 °C
Solidus 1030 °C
Liquidus 1060 °C
Shrinkage 1.6 - 2.1 %Patternmaker's Shrinkage (3/16 to 1/4 in./ft.)
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 260 °CStress-Relieving Temperature
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 92 - 94 %
Lead, Pb 1.0 - 2.0 %
Tin, Sn 1.0 - 2.0 %
Zinc, Zn 2.0 - 6.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Leaded Red Brass, UNS C83600, Copper Casting Alloy (Bronze SAE 40)
Leaded Semi-Red Brass (Valve Metal), UNS C84400, Copper Casting Alloy
Leaded Semi-Red Brass, UNS C84800, Copper Casting Alloy
MetalTek MTEK 85-5-5-5 Cast UNS C83600 Bearing Bronze
Sumitomo Bakelite Durez® 32633 Glass Filled Phenolic, Injection Grade

MC83300b1 / 11899

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.