MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer EXL9414TRC Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN EXL9414TRC resin grade is a 21% PCR(Post Consumer Recycle) contain halogen-free flame retardant polycarbonate featuring transparency, -40 degree C ductility and UL-94 V0 rating for injection molding applications. Excellent impact combined with good flow, all transparent colorability for aesthetics and thin wall flame retardant makes this product an excellent candidate for thin wall applications.

Features: High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Density 1.19 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
Water Absorption at Saturation 0.090 %ISO 62-1
Viscosity 11 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 12 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 54.0 MPa50 mm/min; ISO 527
 56.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 55.0 MPa50 mm/min; ASTM D638
 56.0 MPa50 mm/min; ISO 527
Elongation at Break 95 %50 mm/min; ISO 527
 96 %50 mm/min; ASTM D638
Elongation at Yield 5.4 %50 mm/min; ISO 527
 5.6 %50 mm/min; ASTM D638
Tensile Modulus 2110 MPa50 mm/min; ASTM D638
 2170 MPa1 mm/min; ISO 527
Flexural Strength 86.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2160 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 785 JASTM D256
 311 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 58.0 kJ/m²80*10*3; ISO 180/1A
 34.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 64.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 24.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 65.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 67.0 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 129 °CRate B/50; ISO 306
 135 °CRate A/50; ASTM D1525
UL RTI, Electrical 120 °CUL 746B
UL RTI, Mechanical with Impact 110 °CUL 746B
UL RTI, Mechanical without Impact 120 °CUL 746B
Flammability, UL94 V-2
@Thickness >=1.00 mm
UL 94
 V-0
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 290 - 310 °C
Zone 2 280 - 305 °C
Zone 3 295 - 315 °C
Melt Temperature 295 - 315 °CInjection Molding
Mold Temperature 70.0 - 110 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80245 / 288192

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.