MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer HFD1034 Polycarbonate (PC) (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only

Features: High Flow

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Density 1.20 g/ccASTM D792
 1.20 g/ccISO 1183
Moisture Absorption 0.150 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.30 %ISO 62-1
Viscosity 6.0 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 7.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength at Break 67.0 MPa50 mm/min; ASTM D638
 73.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 58.0 MPa50 mm/min; ASTM D638
 60.0 MPa50 mm/min; ISO 527
Elongation at Break 141 %50 mm/min; ISO 527
 142 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %50 mm/min; ASTM D638
 6.0 %50 mm/min; ISO 527
Tensile Modulus 2080 MPa1 mm/min; ISO 527
 2260 MPa5 mm/min; ASTM D638
Flexural Strength 89.0 MPayield, 2 mm/min; ISO 178
 98.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2070 MPa2 mm/min; ISO 178
 2240 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 966 JASTM D256
 899 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 72.0 kJ/m²80*10*3; ISO 180/1A
 63.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 82.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 69.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 78.0 JASTM D3763
Impact Test 134 JMultiaxial Impact; ISO 6603
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 115 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 115 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 130 °CRate B/50; ISO 306
 131 °CRate B/120; ISO 306
 136 °CRate B/50; ASTM D1525
UL RTI, Electrical 105 °CUL 746B
UL RTI, Mechanical with Impact 105 °CUL 746B
UL RTI, Mechanical without Impact 105 °CUL 746B
Flammability, UL94 HB
@Thickness >=0.800 mm
UL 94
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.582ASTM D542
Haze <= 1.0 %
@Thickness 2.54 mm
ASTM D1003
Transmission, Visible 88 %
@Thickness 2.54 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 255 - 300 °C
Zone 2 250 - 295 °C
Zone 3 260 - 305 °C
Melt Temperature 260 - 305 °CInjection Molding
Mold Temperature 50.0 - 80.0 °C
Drying Temperature 105 - 110 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 24.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00380 - 0.00760 cm
Screw Speed 35 - 75 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80299 / 288246

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.