MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Saint-Gobain CHR® 2254-2 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Categories: Polymer; Adhesive; Tape; Thermoset; Silicone

Material Notes: CHR® 2254 is manufactured from modified PTFE film coated with pressure-sensitive adhesive.

Features/Benefits: Their most outstanding properties are its high dielectric and tensile strength, which make it an extremely durable insulation tape. The high temperature properties of the PTFE and adhesive allow it to perform in continuous temperatures up to 177 °C or 260 °C. A high-modulus tape, they exhibit low elongation which enables it to be applied with automatic wrapping equipment. The other outstanding features include chemical inertness as well as low friction, anti-stick, non-toxic properties and clean release, making it the right material for numerous applications.

Applications: The excellent conformability and release properties of the PTFE backing, along with the high temperature capability of the adhesive, make these tapes ideal for applications such as composite lay-up, roller wrapping, plate masking, heat sealing and other uses where costly clean up is a problem. The aerospace industry can also use these tapes in phase insulation for bundling end turns, spot bundling, anchor breakouts and to protect airframe wire harnesses.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 150 %
Tear Strength 30.0 pliInitial Tear Strength
Peel Strength 0.380 kN/mAdhesion to Steel
 
Electrical PropertiesOriginal ValueComments
Dielectric Breakdown 9000 V
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °F
Minimum Service Temperature, Air -40.0 °F
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Norton® T-100 Virgin Skived PTFE Film (0.010" thick)
Saint-Gobain Norton® Fluorglas® Chemfilm® R167 Extruded Expanded PTFE Film (0.010" thick)
Saint-Gobain CHR® 2045-5 Skived PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Overview of materials for Nylon 66/6
GEHR Plastics Noryl PPO

PSTGQZ352 / 68866

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.