MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound RFL46 Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: LNP LUBRICOMP RFL46 compound is based on Nylon 6/6 resin containing 30% glass fiber, 20% PTFE. Added features of this grade include: Wear Resistant.

Features: Wear resistant,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.54 g/ccASTM D792
Density 1.54 g/ccISO 1183
Water Absorption 0.70 - 0.90 %
@Time 86400 sec
ISO 62-1
Moisture Absorption 0.100 - 0.300 %23°C/50% RH/24 hrs; ISO 62-4
 0.150 - 0.250 %Injection Molding
Moisture Absorption at Equilibrium 0.40 - 0.60 %23°C/50% RH; ISO 62-4
Water Absorption at Saturation 3.8 - 4.1 %ISO 62-1
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.010 - 0.014 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 145 MPa5 mm/min; ISO 527
Elongation at Break 2.5 %5 mm/min; ISO 527
Tensile Modulus 10400 MPa1 mm/min; ISO 527
Flexural Strength 204 MPa1.3 mm/min, 50 mm span; ASTM D790
 213 MPayield, 2 mm/min; ISO 178
Flexural Modulus 8400 MPa1.3 mm/min, 50 mm span; ASTM D790
 8700 MPa2 mm/min; ISO 178
Izod Impact Notched 80.0 JASTM D256
Izod Impact, Unnotched 760 J/mASTM D4812
Izod Impact, Notched (ISO) 9.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²80*10*4; ISO 180/1U
Charpy Impact Unnotched 45.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
Coefficient of Friction, Dynamic 0.59ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.90ASTM D3702 Modified: Manual
K (wear) Factor 16.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 24.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 253 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 262 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 262 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 254 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 251 °CRate B/120; ISO 306
 254 °CRate A/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Zone 2 280 - 295 °C
Zone 3 295 - 305 °C
Melt Temperature 280 - 305 °CInjection Molding
Mold Temperature 95.0 - 110 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80996 / 288943

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.